刘燕,李善吉,许宁斌.丙烯酸铽配合物及其聚合物的制备和性能研究[J].包装工程,2019,40(11):123-128.
LIU Yan,LI Shan-ji,XU Ning-bin.Preparation and Properties of Terbium Acrylate Complex and Its Polymer[J].Packaging Engineering,2019,40(11):123-128.
丙烯酸铽配合物及其聚合物的制备和性能研究
Preparation and Properties of Terbium Acrylate Complex and Its Polymer
投稿时间:2019-02-08  修订日期:2019-06-10
DOI:10.19554/j.cnki.1001-3563.2019.11.018
中文关键词: 丙烯酸  铽配合物  发光性能  热性能
英文关键词: acrylic acid  terbium complex  luminescent property  thermal stability
基金项目:嘉应学院大学生创新创业训练项目(201710582052);广州市教育系统创新学术团队项目(1201610020)
作者单位
刘燕 1.嘉应学院梅州 514015 
李善吉 2.广州工程技术职业学院广州 510075 
许宁斌 1.嘉应学院梅州 514015 
摘要点击次数:
全文下载次数:
中文摘要:
      目的 研究小分子配合物5-丁氧甲基-8-羟基喹啉丙烯酸铽及其与苯乙烯聚合的高分子配合物的发光性能和热性能,并探讨聚合时间对高分子配合物性能的影响。方法 通过氯甲化反应和取代反应合成5-丁氧甲基-8-羟基喹啉(BTMQ),并以BTMQ和丙烯酸(HAA)为配体合成5-丁氧甲基-8-羟基喹啉丙烯酸铽(Tb(BTMQ)2HAA)。然后,用小分子配合物和苯乙烯聚合得高分子配合物p(St-co-Tb(BTMQ)2HAA。通过热重(TG)分析和荧光光谱测试研究配合物的热性能和发光性能。结果 小分子配合物的起始分解温度和荧光强度分别为262 ℃和222;聚合反应为8 h时,高分子配合物的起始分解温度和荧光强度均最大,分别为380 ℃和228。结论 高分子配合物比小分子配合物具有更好的热性能和发光性能,最佳聚合反应时间为8 h。
英文摘要:
      The paper aims to study luminescent property and thermal property of small molecular complex of 5-butyloxymethyl-8-hydroxyquinolin terbium acrylate and its polymer complex with styrene polymer, and discuss effects of polymer time on properties of polymer complex. 5-butyloxymethyl-8- hydroxyl- quinolin (BTMQ) was synthesized by chloromethylation reaction and substitution reaction, and the small molecular complex of 5-butyloxymethyl-8-hydroxyquinolin terbium acrylate (Tb(BTMQ)2HAA) was synthesized with BTMQ and acrylic acid (HAA) as ligands. And then, the polymer complex of p(St-co-Tb(BTMQ)2HAA) was prepared by polymerization of small molecular complex and styrene. The thermal property and luminescent property were investigated by thermogravimetric (TG) analysis and determination of fluorescence spectrum. The initial decomposition temperature and fluorescence intensity of small molecular complex were 262 ℃ and 222 ℃, respectively. When the polymerization time was 8 h, the initial decomposition temperature and fluorescence intensity of the polymer complex were the highest, 380 ℃and 228 ℃, respectively. The Polymer complexes have better thermal and luminescent properties than small molecular complexes. The best polymerization time is 8 h.
查看全文   查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第21282556位访问者    渝ICP备15012534号-2

版权所有:《包装工程》编辑部 2014 All Rights Reserved

邮编:400039 电话:023-68795652 Email: designartj@126.com

    

渝公网安备 50010702501716号